Archive for the “Failure Analysis” Category


Analysis of a Ruptured Inergen Cylinder

Posted on July 3rd, 2019 by Met-Tech

Share This Case Study:

Analysis of a Ruptured Inergen Cylinder SUMMARY: A ruptured Inergen cylinder was received for analysis to determine the cause of failure.  Results indicate the rupture initiated at a longitudinal alignment of several pre-existing axial cracks on the interior of the cylinder.  The pre-existing cracks were characterized by black oxide covered, arc-shaped crack fronts, initiating from […]


Failure Analysis of Corrosion on Stainless Steel Fasteners

Posted on August 1st, 2017 by Met-Tech

Share This Case Study:

  Analysis of CORRODED STAINLESS STEEL BOLTS Summary: Metallurgical Technologies, Inc. (MTi) received five stainless steel bolts from a marine environment. The bolts exhibited corrosion predominantly on the head of the bolt around the set screw, underneath the head of the bolt, and in the threads. MTi was requested to determine the cause of the […]


ANALYSIS OF A CRACKED SPLINE GEAR

Posted on July 1st, 2019 by Met-Tech

Share This Case Study:

ANALYSIS OF A CRACKED SPLINED COUPLING Summary: A fractured spline gear coupling was received for analysis to investigate the cause of failure. Results indicated the coupling fractured in fatigue, initiated at the bottom corner of the keyway from the ID of the coupling. The keyway exhibited significant yielding which widened the keyway, indicating the strength […]


BRASS PLUMBING FITTINGS

Posted on June 7th, 2019 by Met-Tech

Share This Case Study:

ANALYSIS OF DEGRADED BRASS PLUMBING FITTINGS Summary: Two, one-inch, 90° elbow brass plumbing fittings were received for analysis of extensive deterioration and leakage. Results indicated the fittings were severely degraded, due to “plug-type” dezincification corrosion. The dezincification corrosion was due to the high concentration of internal deposits, hot water temperature, water pH and chloride content, […]


Aluminized Steel Heater Tubes

Posted on June 7th, 2019 by Met-Tech

Share This Case Study:

High Temperature Oxidation Failure Of Aluminized Steel Heater Tubes Summary: Two aluminized heater tubes were received for analysis to investigate the cause of failure. Unused tube material also was supplied for comparison. Results indicate that the tubes failed via hot oxidation corrosion at extreme temperatures. Both the heater tube material and processes appear normal. The […]


WELDED STEERING ARM SPINDLE

Posted on June 11th, 2019 by Met-Tech

Share This Case Study:

ANALYSIS OF AN IMPACT FRACTURED, WELDED STEERING ARM SPINDLE ASSEMBLY Summary: A welded left front spindle/steering arm assembly that had fractured at the fillet weld joint between the steering arm and inner brake boss was received for analysis to determine the mode of failure. The intact right front spindle/steering arm was submitted for comparison. Results […]


STEEL PREHEATER TUBE

Posted on June 10th, 2019 by Met-Tech

Share This Case Study:

STRESS CORROSION CRACKING AND INTERGRANULAR CORROSION OF A 316Ti STAINLESS STEEL PREHEATER TUBE Summary: A cracked 316Ti stainless steel preheater tube was analyzed to determine the failure mechanism. A second non-cracked tube section from a different elevation was also analyzed to determine the condition of the tube material. The interior of the tube carries process […]


Corrosion of a Leaking Marine Oil Cooler

Posted on June 13th, 2019 by Met-Tech

Share This Case Study:

Analysis Of Condensate Induced Pitting Corrosion of a Leaking Marine Oil Cooler Summary: Two cores from a marine diesel engine oil cooler were received for analysis to investigate the cause of failure via leaking. Results indicate that the cooler core failed due to pitting corrosion initiated on the interior (oil side) at the edge of […]


Race Car Transmission Input Shaft

Posted on July 1st, 2019 by Met-Tech

Share This Case Study:

  Fatigue Fracture Of A 300M Ultra-high Strength Steel Race Car Transmission Input Shaft Summary: A fractured input shaft used in NASCAR racing was received for analysis to investigate the cause of failure. Results indicate the shaft fractured due to fatigue progression from an intergranular stress crack, initiated at a dot peen identification marking on […]


Fractured Crane Frame Weldment

Posted on July 1st, 2019 by Met-Tech

Share This Case Study:

Analysis Of A Fractured Crane Frame Weldment Summary: A fractured weldment from a crane frame assembly was received for analysis to determine the cause of fracturing along the circumferential fillet weld. Results indicate the fracture occurred by cyclic fatigue crack growth that initiated at the root of the fillet weld due to incomplete penetration by […]


Cracking Of Stainless Steel Nozzle Sleeve

Posted on July 1st, 2019 by Met-Tech

Share This Case Study:

  Fatigue Cracking Of A 316l Stainless Steel Nozzle Sleeve From A Chemical Processing Vessel Corrosion Assisted Fatigue Cracking Of A 316l Stainless Steel Nozzle Sleeve From A Chemical Processing Vessel Summary: A cracked nozzle sleeve stub from a chemical processing vessel of the proprietary vaporizer system was analyzed to determine the cause of cracking. […]


Failed Inconel Condenser Tube

Posted on July 2nd, 2019 by Met-Tech

Share This Case Study:

  Failure Analysis of Failed Inconel Condenser Tube Metallurgical Failure Analysis – Forensic Engineering Metallurgical failure analysis provided by MTi can help minimize and eliminate the extreme effects of unexpected down time in the power industry. We specialize in rapid response with prompt report turnaround. When the root cause of the metal product failure is […]

Tags: , , , , ,


Cracked Nitrided Tool Steel Die Plate

Posted on July 9th, 2019 by Met-Tech

Share This Case Study:

  Failure Analysis of Fractured Tool Steel Die Plate Summary: A cracked polymer filament die plate was received for analysis to determine the cause of cracking. Results indicate the die plate cracked as a result of a brittle nitrided case and an insufficient cross-sectional area of the narrow ligament between the cap screw hole and […]

Tags: , , , , ,


Failure Anaysis Of Ball Bearings

Posted on July 9th, 2019 by Met-Tech

Share This Case Study:

Failure Analysis of Arcing and Contact Fatigue of Ball Bearings Summary: The four seized bearings submitted for metallurgical analysis were determined to have suffered deterioration of their grease to the point that it was inhibiting motion rather than enabling. The grease had turned to a thick (viscous) black sludge that was full of particulate. Electrical […]

Tags: , , ,


Superheater Tube From Boiler

Posted on July 1st, 2019 by Met-Tech

Share This Case Study:

Analysis of T11 Boiler Superheater Tube Rupture SUMMARY: Metallurgical Technologies, Inc. examined a failed superheater tube from XXXXXX X XXX Boiler #7. The ASME SA-213 Grade T11 tube had been in service for 6 to 8 years until failure. The mode of failure was short-term stress rupture due to significant overheating. The microstructure and oxide […]

img23

Failure Analysis Services

Determine cause of failure & recommend ways to prevent future recurrence.

View more
img23

Corrosion Investigation

Determine cause of material degradation that reduces life expectancy.

View more
img23

SEM/EDS
Micro-Analysis

Verify fracture mechanism & initiation. Microstructure composition and imaging.

View more
img23

Metallography Services

Reveals grain structure, thermo mechanical processing & flaw and defect characteristics.

View more